<?xml version="1.0" encoding="UTF-8"?>
<!DOCTYPE article PUBLIC "-//NLM//DTD JATS (Z39.96) Article Authoring DTD v1.4 20240229//EN" "JATS-articleauthoring1.dtd">
<article article-type="research-article" xml:lang="zh-CN" xmlns:xlink="http://www.w3.org/1999/xlink">
  <front>
    <journal-meta>
      <journal-id journal-id-type="publisher-id">28</journal-id>
      <journal-title-group>
        <journal-title>《现代化工技术》原《现代化工》</journal-title>
        <abbrev-journal-title>Modern Chemical Engineering Technology</abbrev-journal-title>
      </journal-title-group>
      <issn>ISSN：3104-770X(P)/3104-7718(O)；原ISSN：2661-3670(P)/2661-3689(O)</issn>
      <publisher>
        <publisher-name>华文国际出版社</publisher-name>
      </publisher>
    </journal-meta>
    <article-meta>
      <article-id pub-id-type="doi">10.12361/2661-3670-07-04-3229</article-id>
      <article-id pub-id-type="publisher-id">14774</article-id>
      <title-group>
        <article-title>硝酸磁力泵隔离套频繁泄漏问题的分析与改进</article-title>
      </title-group>
      <contrib-group>
        <contrib contrib-type="author">
          <string-name>孙国松 （国家能源集团新疆哈密能源化工有限公司）</string-name>
        </contrib>
      </contrib-group>
      <pub-date pub-type="epub">
        <year>2025</year>
        <month>4</month>
      </pub-date>
      <issue>4</issue>
      <abstract>
        <p>本文针对某煤化工企业储运装置 3 台磁力泵硝酸给料泵（2411-P-04A/B）、硝酸卸料泵（2411-P-03）（以下简称硝酸磁力泵）隔离套频繁泄漏问题，通过分析研判历次检维修记录、参照设备运行参数、操作步骤、备品备件质量等原因，发现原隔离套材质哈氏合金 C-276耐 68wt%硝酸溶液腐蚀性低是导致泄漏的主要原因。结合设备厂家提供的腐蚀数据，将隔离套材质更换为钛合金，并优化备品备件采购、验收、维护管理等措施，隔离套使用寿命延长 8 倍有余，有效降低了非计划停机率，提升装置连续运行的稳定性，为下游装置连续供料提供强有力的保障，其中该改进方案《降低磁力泵故障率、提升机泵运行效率》获得该企业五小成果优秀奖，证明了该改进措施的有效性和合理性。</p>
      </abstract>