<?xml version="1.0" encoding="UTF-8"?>
<!DOCTYPE article PUBLIC "-//NLM//DTD JATS (Z39.96) Article Authoring DTD v1.4 20240229//EN" "JATS-articleauthoring1.dtd">
<article article-type="research-article" xml:lang="zh-CN" xmlns:xlink="http://www.w3.org/1999/xlink">
  <front>
    <journal-meta>
      <journal-id journal-id-type="publisher-id">28</journal-id>
      <journal-title-group>
        <journal-title>《现代化工技术》原《现代化工》</journal-title>
        <abbrev-journal-title>Modern Chemical Engineering Technology</abbrev-journal-title>
      </journal-title-group>
      <issn>ISSN：3104-770X(P)/3104-7718(O)；原ISSN：2661-3670(P)/2661-3689(O)</issn>
      <publisher>
        <publisher-name>华文国际出版社</publisher-name>
      </publisher>
    </journal-meta>
    <article-meta>
      <article-id pub-id-type="publisher-id">26474</article-id>
      <title-group>
        <article-title>高温高压化工管道腐蚀机理及防护措施研究</article-title>
      </title-group>
      <contrib-group>
        <contrib contrib-type="author">
          <string-name>秦向辉 中国五环工程有限公司</string-name>
        </contrib>
      </contrib-group>
      <pub-date pub-type="epub">
        <year>2026</year>
        <month>1</month>
      </pub-date>
      <issue>1</issue>
      <abstract>
        <p>高温高压化工管道是石油化工、煤化工、精细化工等流程工业的核心承压部件，长期服役于高温、高压、强腐蚀介质耦合工况，易发生氧化、硫化、氢蚀、应力腐蚀、点蚀等多种失效形式，严重威胁装置安全稳定运行。本文系统阐述高温高压化工管道的典型腐蚀机理，分类剖析均匀腐蚀、局部腐蚀、应力腐蚀、氢致腐蚀等失效类型，明确温度、压力、介质成分、材料组织、流速与应力等关键影响因素；从材料选型、表面防护、工艺控制、电化学保护、缓蚀剂应用、检测运维六个维度提出全流程防护技术体系；结合工程案例给出典型工况防护方案，为高温高压管道长周期安全运行提供理论依据与技术参考。</p>