<?xml version="1.0" encoding="UTF-8"?>
<!DOCTYPE article PUBLIC "-//NLM//DTD JATS (Z39.96) Article Authoring DTD v1.4 20240229//EN" "JATS-articleauthoring1.dtd">
<article article-type="research-article" xml:lang="zh-CN" xmlns:xlink="http://www.w3.org/1999/xlink">
  <front>
    <journal-meta>
      <journal-id journal-id-type="publisher-id">4</journal-id>
      <journal-title-group>
        <journal-title>学习导刊</journal-title>
        <abbrev-journal-title>Learning Guide</abbrev-journal-title>
      </journal-title-group>
      <issn>ISSN:3104-4905（Print）（原2972-418X）</issn>
      <publisher>
        <publisher-name>华文科学出版社（HUAWEN SCIENCE PRESS）</publisher-name>
      </publisher>
    </journal-meta>
    <article-meta>
      <article-id pub-id-type="publisher-id">9113</article-id>
      <title-group>
        <article-title>聚乳酸/纳米粘土复合材料生物降解性能效果</article-title>
      </title-group>
      <contrib-group>
        <contrib contrib-type="author">
          <string-name>方正予 丁时蒸 （悉尼大学 241000）</string-name>
        </contrib>
      </contrib-group>
      <pub-date pub-type="epub">
        <year>2024</year>
        <month>12</month>
      </pub-date>
      <issue>12</issue>
      <abstract>
        <p>摘要：目的：本研究旨在评估聚乳酸/纳米粘土复合材料在不同环境条件下的生物降解性能，方法：将聚乳酸和聚乳酸/
纳米粘土复合材料样品（各 50 个）在 37℃、50%湿度条件下进行为期 12 周的降解实验，并分别模拟体内环境，通过测量质
量损失率、扫描电子显微镜（SEM）观察表面形态变化、傅里叶变换红外光谱（FTIR）和 X 射线衍射（XRD）分析实验组的化
学结构和结晶度变化来评估降解性能。结果：在第 1、4、12 周时，对照组聚乳酸的平均质量损失率分别为 2.31±0.52%、
8.93±1.24%和 25.05±2.06%，而实验组聚乳酸/纳米粘土复合材料的平均质量损失率分别为 2.11±0.42%、7.23±1.04%和
20.55±1.86%，实验组质量损失率低于对照组，P</p>
      </abstract>